The determination is carried out by pyrolysis of a test portion at 550 °C in nitrogen followd by a calcination in a muffle furnace at 900 °C. The carbon black content is calculated from difference in mass before and after calcination. When so determined the carbon black content in polyethylen pipe material shall be 2,5 0,5 % (m/m).
ПОВУЧЕН
ISO 6964:1986
95.99
Повучен
27. 2. 2019.
ОБЈАВЉЕН
ISO 6964:2019
Poliolefinske cevi i fitinzi - Određivanje sadržaja čađi žarenjem i razlaganjem - Metoda ispitivanja i osnovna specifikacija - (Identičan sa ISO 6964:1986)