This document specifies the dimensions, the method of sampling and the preparation of the test specimens, also the conditions for performing the low temperature tensile test perpendicular to the weld in order to determine the low temperature tensile welding factor.
A low temperature tensile test can be used in conjunction with other tests (e.g. bend, tensile creep, macro) to assess the performance of welded assemblies, made from thermoplastics materials.
The low temperature tensile welding factor and the appearance of the fracture surface provide a guide regarding the ductility of the joint and the quality of the work.
This document is applicable to co-axial or co-planar welded assemblies made from thermoplastics materials filled or unfilled, but not reinforced, irrespective of the welding process used.
This document does not apply to co-axial welded assemblies of an external diameter less than 20 mm.
PUBLISHED
SRPS EN 12814-6:2012
PROJECT
dnaSRPS EN 12814-6:2024
50.20
Proof sent to secretariat or FDIS ballot initiated: 8 weeks
Apr 30, 2026
To view the full content, you need to register or to log in to your account by clicking on the "Log in" button