Phone: (011) 7541-421, 3409-301, 3409-335, 6547-293, 3409-310
E-mail: Standards sales: prodaja@iss.rs Education: iss-edukacija@iss.rs Information about standards: infocentar@iss.rs
Stevana Brakusa 2, 11030 Beograd
Main menu

naSRPS EN 12390-12:2024

Testing of hardened concrete - Part 12: Determination of the carbonation resistance of concrete - Accelerated carbonation method

General information

40.10     Aug 18, 2025

40.20    Oct 16, 2025

ISS

U071

European Norm

91.100.30  

English  

Scope

This document describes a method for evaluating the carbonation resistance of concrete using test conditions that accelerate carbonation. After a defined period of curing and a period of preconditioning, the test is carried out under controlled exposure conditions using an increased level of carbon dioxide.
NOTE The test performed under reference conditions takes a minimum of 112 days comprising a minimum age of the specimen prior to curing under water of 28 days, a minimum preconditioning period of 14 days and an exposure period to increased carbon dioxide level of 70 days.
This procedure is not a method for the determination of carbonation depths in existing concrete structures.

Life cycle

PREVIOUSLY

PUBLISHED
SRPS EN 12390-12:2020

NOW

PROJECT
naSRPS EN 12390-12:2024
40.10 harmonizedStageCodeLabel.40.10
Aug 18, 2025

Related project

Adopted from prEN 12390-12 IDENTICAL