SRPS CEN/TS 12390-10:2008

Testing hardened concrete - Part 10: Determination of the relative carbonation resistance of concrete

Dec 29, 2008
95.99   Withdrawal of Standard   Jun 24, 2019

General information

95.99     Jun 24, 2019

ISS

U071

Technical Specification

91.100.30  

English  

Buying

Withdrawn

Language in which you want to receive the document.

Scope

This is a method for evaluating the carbonation resistance of concrete mixes by comparison with a concrete mix with known carbonation resistance. It is not a method for the determination of carbonation depths in existing concrete structures. The test is carried out under controlled exposure conditions using natural levels of carbon dioxide or under natural conditions protected from direct rainfall.
If the carbonation depth of the unknown mix is equal or less than the known mix, it is be assumed that the risk of reinforcement corrosion for the new mix is equivalent to the known mix (with the same cover required for the known mix). The “reference” concrete may be any concrete with known performance in the intended place of use (environment).

Related directives

NOTE: If the word "harmonized" (marked in green) is not found in the field with the name of the directive, it means that the European standard is not cited in the OJEU.

89/106/EEC

Construction products

305/2011

Regulation (eu) No 305/2011 of the European Parliament and of the Council of 9 march 2011 laying down harmonised conditions for the marketing of construction products and repealing council directive 89/106/eec

Life cycle

NOW

WITHDRAWN
SRPS CEN/TS 12390-10:2008
95.99 Withdrawal of Standard
Jun 24, 2019

REVISED BY

PUBLISHED
SRPS EN 12390-10:2019

Related project

Adopted from CEN/TS 12390-10:2007