This standard specifies the electrolytic cadmium plating of parts in steels of tensile strength Rm (max.) </= 1450 MPa, copper, copper alloys and nickel alloys, the temperature in service of which does not exceed 235 °C. This standardd is applicable whenever referenced.
WITHDRAWN
SRPS EN 2133:2009
95.99
Withdrawal of Standard
Apr 30, 2014
WITHDRAWN
SRPS EN 2133:2014