In the test to determine the tensile strenght of thermally sprayed deposits, the specimen is loaded in tension. The test is conducted to obtain information on the strength of the coating and/or the strength of the bond between the spary deposit and the parent metal.
WITHDRAWN
SRPS EN 582:2010
95.99
Withdrawal of Standard
Aug 31, 2017
PUBLISHED
SRPS EN ISO 14916:2017