This European Standard specifies Vignole railway rails of 46 kg/m and greater linear mass, for general and high speed railway track usage.
Seven pearlitic steel grades are specified covering a hardness range of 200 to 390 HBW and include non heat treated carbon manganese steels; non heat treated alloy steels; and heat treated carbon manganese and low alloy steels.
There are 21 rail profiles specified in this Standard.
Two classes of rail straightness are specified, differing in requirements for straightness, surface flatness and crown profile. Two classes of profile tolerances are specified.
NOTE: If the word "harmonized" (marked in green) is not found in the field with the name of the directive, it means that the European standard is not cited in the OJEU.
Procurement procedures of entities operating in the water, energy, transport and telecommunications sectors
Interoperability of the trans-European high-speed rail system
Harmonized
                    WITHDRAWN
                    SRPS EN 13674-1:2010
                    95.99
                                        Withdrawal of Standard
                    Sep 30, 2011
                
                WITHDRAWN
                                    SRPS EN 13674-1:2011
                            
ДИРЕКЦИЈА ЗА ЖЕЛЕЗНИЦЕ